Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 582 °C | 1080 °F | Flow Point |
Lucas-Milhaupt AL 718 Aluminum Brazing Filler Metal Applications:AL 718 filler metal is generally used to join aluminum and aluminum alloys. It can be used to join titanium or aluminum to dissimilar metals. When joining to dissimilar metals thought.. |
|||
Liquidus | 582 °C | 1080 °F | |
Solvay Chemicals NOCOLOK® Braze Paste x47-12 A braze paste specifically formulated for providing viscous mixture of flux and alloy for brazing noncladded aluminum materials. Paste can be dispensed manually by brush, syringe, or with automatic .. |