Solvay Chemicals NOCOLOK® Braze Paste x47-12

Category Fluid
Manufacturer Solvay Chemicals
Trade Name NOCOLOK®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals NOCOLOK® Braze Paste x47-12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A braze paste specifically formulated for providing viscous mixture of flux and alloy for brazing noncladded aluminum materials. Paste can be dispensed manually by brush, syringe, or with automatic dispensing equipment. Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical AppliancesInformation provided by Solvay
Mechanical Properties Metric English Comments
Tensile Strength 24.1 MPa
3500 psi
Thermal Properties Metric English Comments
Melting Point 577 - 582 °C
1070 - 1080 °F
Solidus 577 °C
1070 °F
Liquidus 582 °C
1080 °F
Component Elements Properties Metric English Comments
Aluminum, Al 86.85 - 89 %
86.85 - 89 %
Silicon, Si 11 - 13 %
11 - 13 %
Descriptive Properties Value Comments
Appearance silver grey
Composition >0.15%
Others Total