Polymer Property : Liquidus = 1080 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 582 °C
1080 °F
Flow Point
Lucas-Milhaupt AL 718 Aluminum Brazing Filler Metal
Applications:AL 718 filler metal is generally used to join aluminum and aluminum alloys. It can be used to join titanium or aluminum to dissimilar metals. When joining to dissimilar metals thought..
Liquidus 582 °C
1080 °F
Solvay Chemicals NOCOLOK® Braze Paste x47-12
A braze paste specifically formulated for providing viscous mixture of flux and alloy for brazing noncladded aluminum materials. Paste can be dispensed manually by brush, syringe, or with automatic ..