Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 950 °C | 1740 °F | |
Indium Corp. Indalloy 196 Gold Solder Alloy Information Provided by Indium Corporation |
|||
Liquidus | 950 °C | 1740 °F | |
Wieland 1601 Wilaform Gold Soft yellow gold alloy, ideally for the production of strongly deformed parts in decoration manufacturing and for metal coinage.Applications: casting, chains, coin/shape, laminar decoration, pipes, .. |
|||
Liquidus | 949 °C | 1740 °F | |
Williams Advanced Alloys Wambraze™ WB949 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |
|||
Liquidus | 950 °C | 1740 °F | |
Williams Advanced Alloys Wambraze™ WB950 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |