Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy 196 Gold Solder Alloy

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 196 Gold Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 15.92 g/cc
0.5751 lb/in³
Thermal Properties Metric English Comments
Melting Point 950 °C
1740 °F
Eutectic
Solidus 950 °C
1740 °F
Liquidus 950 °C
1740 °F
Component Elements Properties Metric English Comments
Gold, Au 82 %
82 %
Nickel, Ni 18 %
18 %
Users viewing this material also viewed the following: