Polymer Property : Liquidus = 1385 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 1385 °C
2525 °F
Special Metals INCOLOY® Alloy 800
A nickel-iron-chromium alloy with good strength and excellent resistance to oxidation and carburization in high-temperature atmospheres. It also resists corrosion by many aqueous environments. The..
Liquidus 1385 °C
2525 °F
Special Metals INCOLOY® Alloy 800HT™
A nickel-iron-chromium alloy having the same basic composition as INCOLOY alloy 800 but with significantly higher creep-rupture strength. The higher strength results from close control of the carbo..
Liquidus 1385 °C
2525 °F
Carlson C 800 Nickel-Iron-Chromium Alloy
General DescriptionCarlson Alloy C 800 is a nickel-iron-chromium alloy, combining high strength with excellent resistance to oxidation and carburization at elevated temperatures. This alloy resists..
Liquidus 1385 °C
2525 °F
Carlson C 800AT Nickel-Iron-Chromium Alloy
General DescriptionCarlson Alloy C 800AT is a modification of Carlson Alloy C 800, exhibiting higher creep and rupture strengths. This nickel-iron-chromium alloy has a carbon content restricted to ..
Liquidus 1385 °C
2525 °F
ATI Allegheny Ludlum Type 332 Stainless Steel, UNS N08800
Type 332 is a nickel and chromium austenitic stainless steel designed to resist oxidation and carburization at elevated temperatures. The nickel content, 32%, makes the alloy highly resistant both ..
Liquidus 1385 °C
2525 °F
Carlson C 800H Nickel-Iron-Chromium Alloy
General DescriptionCarlson Alloy C 800 is a nickel-iron-chromium alloy, combining high strength with excellent resistance to oxidation and carburization at elevated temperatures. This alloy resists..