Special Metals INCOLOY® Alloy 800

Category Metal , Superalloy , Iron Base
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name INCOLOY®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals INCOLOY® Alloy 800.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A nickel-iron-chromium alloy with good strength and excellent resistance to oxidation and carburization in high-temperature atmospheres. It also resists corrosion by many aqueous environments. The alloy maintains a stable, austenitic structure during prolonged exposure to high temperatures. Used for process piping, heat exchangers, carburizing equipment, heating-element sheathing, and nuclear steam-generator tubing. Standard product forms are round, flats, forging stock, pipe, tube, plate, sheet, strip, and wire.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 7.94 g/cc
0.287 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 600 MPa
87000 psi
Annealed
500 MPa

@Temperature 550 °C
72500 psi

@Temperature 1020 °F
Annealed prior to test
Tensile Strength, Yield 275 MPa
39900 psi
Annealed
213 MPa

@Temperature 550 °C
30900 psi

@Temperature 1020 °F
Annealed prior to test
Elongation at Break 45 %
45 %
Annealed prior to test.
35 %

@Temperature 550 °C
35 %

@Temperature 1020 °F
Annealed prior to test.
Thermal Properties Metric English Comments
CTE, linear 14.4 µm/m-°C

@Temperature 20.0 - 100 °C
8.00 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.460 J/g-°C
0.110 BTU/lb-°F
Thermal Conductivity 11.5 W/m-K
79.8 BTU-in/hr-ft²-°F
Melting Point 1357 - 1385 °C
2475 - 2525 °F
Solidus 1357 °C
2475 °F
Liquidus 1385 °C
2525 °F
Component Elements Properties Metric English Comments
Aluminum, Al 0.15 - 0.60 %
0.15 - 0.60 %
Carbon, C <= 0.10 %
<= 0.10 %
Chromium, Cr 19 - 23 %
19 - 23 %
Copper, Cu <= 0.75 %
<= 0.75 %
Iron, Fe >= 39.5 %
>= 39.5 %
Manganese, Mn <= 1.5 %
<= 1.5 %
Nickel, Ni 30 - 35 %
30 - 35 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.015 %
<= 0.015 %
Titanium, Ti 0.15 - 0.60 %
0.15 - 0.60 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000989 ohm-cm
0.0000989 ohm-cm
Magnetic Permeability 1.014
1.014
at 200 oersted (15.9 kA/m)
Curie Temperature -115 °C
-175 °F