Thermal Properties Metric English Comments
Liquidus 1370 °C
2500 °F
Haynes HR-160® alloy plate, aged 1000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Liquidus 1370 °C
2500 °F
Haynes HR-160® alloy plate, aged 4000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Liquidus 1370 °C
2500 °F
Haynes HR-160® alloy, annealed plate
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Liquidus 1370 °C
2500 °F
Haynes HR-160® alloy, plate, aged 1000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Liquidus 1370 °C
2500 °F
Haynes HR-160® alloy, plate, aged 1000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Liquidus 1370 °C
2500 °F
Haynes HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Liquidus 1370 °C
2500 °F
Haynes HR-160® alloy, plate, aged 4000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Liquidus 1370 °C
2500 °F
Haynes HR-160® alloy, plate, aged 8000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Liquidus 1370 °C
2500 °F
Haynes HR-160® alloy, plate, aged 8000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Liquidus 1370 °C
2500 °F
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Liquidus 1370 °C
2500 °F
HP Alloys Alloy C-276, 10% Cold Worked
10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Liquidus 1370 °C
2500 °F
HP Alloys Alloy C-276, 20% Cold Worked
20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Liquidus 1370 °C
2500 °F
HP Alloys Alloy C-276, 40% Cold Worked
40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Liquidus 1370 °C
2500 °F
HP Alloys Alloy C-276, 50% Cold Worked
50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Liquidus 1370 °C
2500 °F
Special Metals INCONEL® Alloy C-276
A nickel-molybdenum-chromium alloy with an addition of tungsten having excellent corrosion resistance in a wide range of severe environments. The high molybdenum content makes the alloy especially ..
Liquidus 1370 °C
2500 °F
Special Metals INCONEL® C276 Nickel Superalloy Bar
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed bar. Other property values are typical of INCO® C276.Data provided by the manufacturer, Special ..
Liquidus 1370 °C
2500 °F
Special Metals INCONEL® C276 Nickel Superalloy Plate
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed plate. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia..
Liquidus 1370 °C
2500 °F
Special Metals INCONEL® C276 Nickel Superalloy Sheet
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed sheet. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia..
Liquidus 1370 °C
2500 °F
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 0% Cold Work (Annealed)
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed tubing. Other property values are typical of INCO® C276.Data provided by the manufacturer, Speci..
Liquidus 1370 °C
2500 °F
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 24% Cold Work
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 24% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m..
Liquidus 1370 °C
2500 °F
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 27% Cold Work
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 27% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m..
Liquidus 1370 °C
2500 °F
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 30% Cold Work
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 30% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m..
Liquidus 1370 °C
2500 °F
Special Metals NIMONIC® Alloy 90
A precipitation-hardenable nickel-chromium-cobalt alloy having high stress-rupture strength and creep resistance at temperatures to about 1700°F (920°C). The alloy also has good resistance to..
Liquidus 1370 °C
2490 °F
Weartech International WT-21 Cobalt Hardfacing & Wear Resistant Alloy
Applications: hot trimming & forging dies, high pressure high temperature valves, hot shears, valve seats, pump impellers, ringsInformation provided by Weartech International
Liquidus 1370 °C
2500 °F
Carlson GOC 276 Nickel-Molybdenum-Chromium
General DescriptionCarlson Alloy GOC 276 is a nickel-molybdenum-chromium alloy exhibiting outstanding corrosion resistance over a wide range of service environments. This alloy is generally use in ..
Liquidus 1370 °C
2500 °F
HP Alloys Alloy C-276, 30% Cold Worked
30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..