Polymer Property : Solidus = 96.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 96.0 °C
205 °F
Indium Corp. Indalloy 105 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Solidus 96.0 °C
205 °F
Indium Corp. Indalloy 72 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Solidus 96.0 °C
205 °F
Indium Corp. Indalloy 74 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Solidus 96.0 °C
205 °F
Indium Corp. Indalloy 81 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Solidus 96.0 °C
205 °F
Indium Corp. Indalloy 83 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Solidus 96.0 °C
205 °F
Indium Corp. Indalloy 85 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Solidus 96.0 °C
205 °F
Indium Corp. Indalloy® 42 Bi-Sn-Pb Solder Alloy
Bismuth added to achieve a low melting point. Fair wettability.Information provided by the manufacturer, Indium Corporation.
Solidus 96.0 °C
205 °F
Indium Corp. Indalloy 49 Bismuth Solder Alloy
Information Provided by Indium Corporation
Solidus 96.0 °C
205 °F
Williams Advanced Alloys WS96 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Solidus 96.0 °C
205 °F
Indium Corp. Indalloy 39 Bismuth Solder Alloy
Low temperature eutectic solder. Can be used on the same metallization as SnPb based solders. Lowest temperature solder pasteInformation Provided by Indium Corporation