Indium Corp. Indalloy 81 Bismuth-Lead-Tin Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 81 Bismuth-Lead-Tin Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.43 g/cc
0.341 lb/in³
Thermal Properties Metric English Comments
Melting Point 96.0 - 137 °C
205 - 279 °F
Solidus 96.0 °C
205 °F
Liquidus 137 °C
279 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 28.5 %
28.5 %
Lead, Pb 43 %
43 %
Tin, Sn 28.5 %
28.5 %