Williams Advanced Alloys WS96 Solder

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Williams Advanced Alloys
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Williams Advanced Alloys WS96 Solder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 9.58 g/cc
0.346 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 22.1 MPa
3200 psi
Thermal Properties Metric English Comments
CTE, linear 38.0 µm/m-°C

@Temperature 20.0 °C
21.1 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 15.0 W/m-K
104 BTU-in/hr-ft²-°F
Melting Point 96.0 °C
205 °F
Solidus 96.0 °C
205 °F
Liquidus 96.0 °C
205 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 52 %
52 %
Lead, Pb 30 %
30 %
Tin, Sn 18 %
18 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00005375 ohm-cm
0.00005375 ohm-cm