Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucas-Milhaupt Silvalite Brazing Alloy

Category Metal , Nonferrous Metal , Copper Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name Silvalite
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt Silvalite Brazing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SILVALITE is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on vibration free joints. It is very effective for joining tight fitting copper pipe and tubing. SILVALITE should not be used on ferrous metals or copper alloys containing more than 10% nickel because of phosphorus embrittlement due to reactions with iron or nickel. Its melting characteristics are such that on the low end of its brazing temperature range it has “sluggish” flow characteristics which enable it to fill gaps better, making it ideal for loose-fitting joints. On the other hand, when brazing at high end of its brazing temperature range, it is very fluid, making ideal for tight-fitting joints required deep penetration. Melting of SILVALITE is virtually complete at 1350°F (732°C). Best results are obtained when brazing slightly above this temperature.Applications:The phosphorous content of SILVALITE acts as a fluxing agent and no flux is necessary when brazing copper to copper joints. However, when used with a copper alloy or one of the other brazeable metals, a brazing flux must be used to promote wetting, bonding, and flow throughout the joint. The flow point of SILVALITE is 1350°F (732°C).Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Specific Gravity 7.986 g/cc
7.986 g/cc
Density 8.00 g/cc
0.289 lb/in³
Thermal Properties Metric English Comments
Melting Point 643 - 799 °C
1190 - 1470 °F
Solidus 643 °C
1190 °F
Liquidus 799 °C
1470 °F
Maximum Service Temperature, Air 149 °C
300 °F
continuous
204 °C
400 °F
intermittent
Component Elements Properties Metric English Comments
Copper, Cu 91.15 - 92.1 %
91.15 - 92.1 %
As balance
Other, total <= 0.15 %
<= 0.15 %
Phosphorous, P 6.6 - 7.0 %
6.6 - 7.0 %
Silver, Ag 1.3 - 1.7 %
1.3 - 1.7 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000315 ohm-cm
0.0000315 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 732 - 799 °C
1350 - 1470 °F
Brazing Temperature
Descriptive Properties Value Comments
Color Light Copper
Electrical Conductivity (% IACS) 5.5
Users viewing this material also viewed the following: