Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Williams Advanced Alloys WS181 Solder

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy , Tin Alloy
Manufacturer Williams Advanced Alloys
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Williams Advanced Alloys WS181 Solder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 8.42 g/cc
0.304 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 36.3 MPa
5260 psi
Thermal Properties Metric English Comments
CTE, linear 23.0 µm/m-°C

@Temperature 20.0 °C
12.8 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 23.0 W/m-K
160 BTU-in/hr-ft²-°F
Melting Point 134 - 181 °C
273 - 358 °F
Solidus 134 °C
273 °F
Liquidus 181 °C
358 °F
Component Elements Properties Metric English Comments
Indium, In 25 %
25 %
Lead, Pb 37.5 %
37.5 %
Tin, Sn 37.5 %
37.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00002205 ohm-cm
0.00002205 ohm-cm