Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 179 °C | 354 °F | |
Indium Corp. Indalloy 127 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 179 °C | 354 °F | |
Indium Corp. Indalloy 142 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 179 °C | 354 °F | |
Indium Corp. Indalloy 154 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 179 °C | 354 °F | |
Indium Corp. Indalloy 210 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 179 °C | 354 °F | |
Indium Corp. Indalloy® Sn62 Sn-Pb-Ag Solder Alloy Good general purpose solder. Can be used on silver bearing surfaces to reduce scavenging.Information provided by the manufacturer, Indium Corporation. |
|||
Solidus | 179 °C | 354 °F | |
Indium Corp. Indalloy 104 Tin-Lead Solder Alloy Widely used electronic solder. Good for silver metallization. Has improved strength and fatigue propertiesInformation Provided by Indium Corporation |
|||
Solidus | 179 °C | 354 °F | |
Indium Corp. Indalloy 137 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 179 °C | 354 °F | |
Williams Advanced Alloys WS179 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Solidus | 179 °C | 354 °F | |
AIM 62Sn/Pb36/Ag2 Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |