Indium Corp. Indalloy 154 Tin-Lead Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 154 Tin-Lead Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.26 g/cc
0.335 lb/in³
Thermal Properties Metric English Comments
Melting Point 179 - 289 °C
354 - 552 °F
Solidus 179 °C
354 °F
Liquidus 289 °C
552 °F
Component Elements Properties Metric English Comments
Lead, Pb 57 %
57 %
Silver, Ag 3.0 %
3.0 %
Tin, Sn 40 %
40 %