Solidus 577 °C
1070 °F
Indium Corp. Indalloy 191 Aluminum Solder Alloy
Information Provided by Indium Corporation
Solidus 577 °C
1070 °F
Melting Point
Lucas-Milhaupt AL 718 Aluminum Brazing Filler Metal
Applications:AL 718 filler metal is generally used to join aluminum and aluminum alloys. It can be used to join titanium or aluminum to dissimilar metals. When joining to dissimilar metals thought..
Solidus 577 °C
1070 °F
Solvay Chemicals NOCOLOK® Braze Paste x43-7
A braze paste specifically formulated for providing viscous mixture of flux and alloy for brazing noncladded aluminum materials, including 1100, 3001 and 6061 series aluminum. Uses: Automotive Sect..
Solidus 577 °C
1070 °F
Solvay Chemicals NOCOLOK® Braze Paste x47-12
A braze paste specifically formulated for providing viscous mixture of flux and alloy for brazing noncladded aluminum materials. Paste can be dispensed manually by brush, syringe, or with automatic ..
Solidus 577 °C
1070 °F
Solvay Chemicals NOCOLOK® Braze Paste x45-10
NOCOLOK® Braze Paste X45-10 is specifically formulated for providing viscous mixture or flux and alloy for brazing noncladded aluminum materials. Uses: Automotive Sector, Commercial & Residentia..
Solidus 577 °C
1070 °F
Indium Corp. Indalloy 188 Aluminum Solder Alloy
Information Provided by Indium Corporation
Solidus 577 °C
1070 °F
Indium Corp. Indalloy 190 Aluminum Solder Alloy
Information Provided by Indium Corporation