Material Notes:
A braze paste specifically formulated for providing viscous mixture of flux and alloy for brazing noncladded aluminum materials, including 1100, 3001 and 6061 series aluminum. Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical AppliancesInformation provided by Solvay
Mechanical Properties Metric English Comments
Tensile Strength 24.1 MPa
3500 psi
Thermal Properties Metric English Comments
Melting Point 577 - 613 °C
1070 - 1140 °F
Solidus 577 °C
1070 °F
Liquidus 613 °C
1140 °F
Component Elements Properties Metric English Comments
Aluminum, Al 92.25 - 93.5 %
92.25 - 93.5 %
Silicon, Si 6.5 - 7.5 %
6.5 - 7.5 %
Descriptive Properties Value Comments
Appearance silver grey
Composition >0.15%
Others Total