Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.20 W/m-K @Temperature 100 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 42 Dense Refractory Brick Description: Because of its abrasion resistance and high density, this brick performs very well in rotary cement kilns.Remarks: This data represents average values, obtained from samples that were c.. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 650 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast B Sp Dense Refractory Brick Description: A very dense brick, high resistance against slag penetration. Application: in rotary kilns (cement) and incinerators.Remarks: This data represents average values, obtained from samples .. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 1100 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast C Dense Refractory Brick Description: A dry-pressed fireclay brick for use up to 1250°C with a good resistance to acid slags and vapors. Application: industrial furnaces, chimneys, electrolytic reduction cells.Remarks: T.. |
|||
Thermal Conductivity | 1.20 - 1.30 W/m-K @Temperature 1300 °C |
8.33 - 9.02 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast FLUCON 140 Dense Self Flowing Refractory Castable Description: Flucon 140 is a self flowing low cement castable, based on a high quality chamotte grog.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 1.20 - 1.30 W/m-K @Temperature 1000 °C |
8.33 - 9.02 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast VIBRON 140 C RAPID Dense Vibrating Refractory Castable Description: Vibron 140 C Rapid is a low cement castable, based on high quality coarse chamotte grog. Because of special additives this castable is special suited for a faster heating schedule.Remar.. |
|||
Thermal Conductivity | 1.20 - 1.30 W/m-K @Temperature 1300 °C |
8.33 - 9.02 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast VIBRON 140 Dense Vibrating Refractory Castable Description: Vibron 140 is a low cement castable, based on high quality chamotte.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 1.20 - 1.30 W/m-K @Temperature 100 °C |
8.33 - 9.02 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 160 Dense Vibrating Refractory Castable Description: Vibron 160 is a low cement vibrating castable on andalusite base, characterized by a high strength and excellent thermal shock resistance.Remarks: Indicated values apply to vibrated pro.. |
|||
Thermal Conductivity | 1.20 - 1.30 W/m-K @Temperature 100 °C |
8.33 - 9.02 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 160 H Dense Vibrating Refractory Castable Description: Vibron 160 H is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance.Remarks: Indicated values apply to vib.. |
|||
Thermal Conductivity | 1.20 - 1.30 W/m-K @Temperature 100 °C |
8.33 - 9.02 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 165 Dense Vibrating Refractory Castable Description: Vibron 165 is a low cement castable based on andalusite and especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provide.. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 100 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast A 1 S Dense Refractory Brick Description: A brick with a high creep resistance, successfully applied in anode baking furnaces and in the transition zone of rotary cement kilns.Remarks: This data represents average values, obtai.. |
|||
Thermal Conductivity | 1.20 - 1.30 W/m-K @Temperature 100 °C |
8.33 - 9.02 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 160 H RAPID Dense Vibrating Refractory Castable Description: Vibron 160 H Rap is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance. Because of special additives, thi.. |
|||
Thermal Conductivity | 1.20 W/m-K @Temperature 600 °C |
8.33 BTU-in/hr-ft²-°F @Temperature 1110 °F |
EN 993-15 1998 |
Skamol Group SKAMOBAR 69 Low-Alumina Fireclay Brick Low-alumina fireclay brick has the following characteristics: Max. service temperature 1100°C (2012°F)For barrier lining of aluminum reduction cellsExcellent cryolite resistanceLow thermal con.. |