Material Notes:
Description: A very dense brick, high resistance against slag penetration. Application: in rotary kilns (cement) and incinerators.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 2.20 g/cc
0.0795 lb/in³
Apparent
Porosity 14 %
14 %
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 60.0 MPa
8700 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.05 W/m-K

@Temperature 100 °C
7.29 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.20 W/m-K

@Temperature 650 °C
8.33 BTU-in/hr-ft²-°F

@Temperature 1200 °F
1.35 W/m-K

@Temperature 1100 °C
9.37 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Maximum Service Temperature, Air 1300 °C
2370 °F
1350 °C
2460 °F
Deformation under load - t<sub>a</sub>
Component Elements Properties Metric English Comments
Al2O3 35 %
35 %
Fe2O3 <= 2.0 %
<= 2.0 %
SiO2 58 %
58 %
Descriptive Properties Value Comments
Segercone 31
Thermal Shock Resistance 5 cycles