Thermal Properties Metric English Comments
Thermal Conductivity 1.10 - 1.30 W/m-K

@Temperature 600 °C
7.63 - 9.02 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 60 S Moldable Refractory Material
Description: Because this material contains a high percentage of sillimanite, it has a very good thermal shock resistance together with a very good slag resistance. Therefore this material finds its..
Thermal Conductivity 1.20 - 1.30 W/m-K

@Temperature 1300 °C
8.33 - 9.02 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast FLUCON 140 Dense Self Flowing Refractory Castable
Description: Flucon 140 is a self flowing low cement castable, based on a high quality chamotte grog.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Thermal Conductivity 1.20 - 1.30 W/m-K

@Temperature 1000 °C
8.33 - 9.02 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast VIBRON 140 C RAPID Dense Vibrating Refractory Castable
Description: Vibron 140 C Rapid is a low cement castable, based on high quality coarse chamotte grog. Because of special additives this castable is special suited for a faster heating schedule.Remar..
Thermal Conductivity 1.20 - 1.30 W/m-K

@Temperature 1300 °C
8.33 - 9.02 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast VIBRON 140 Dense Vibrating Refractory Castable
Description: Vibron 140 is a low cement castable, based on high quality chamotte.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Thermal Conductivity 1.20 - 1.30 W/m-K

@Temperature 100 °C
8.33 - 9.02 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 160 Dense Vibrating Refractory Castable
Description: Vibron 160 is a low cement vibrating castable on andalusite base, characterized by a high strength and excellent thermal shock resistance.Remarks: Indicated values apply to vibrated pro..
Thermal Conductivity 1.20 - 1.30 W/m-K

@Temperature 100 °C
8.33 - 9.02 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 160 H Dense Vibrating Refractory Castable
Description: Vibron 160 H is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance.Remarks: Indicated values apply to vib..
Thermal Conductivity 1.20 - 1.30 W/m-K

@Temperature 100 °C
8.33 - 9.02 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 165 Dense Vibrating Refractory Castable
Description: Vibron 165 is a low cement castable based on andalusite and especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provide..
Thermal Conductivity 1.20 - 1.30 W/m-K

@Temperature 100 °C
8.33 - 9.02 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 160 H RAPID Dense Vibrating Refractory Castable
Description: Vibron 160 H Rap is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance. Because of special additives, thi..