Thermal Properties Metric English Comments
Thermal Conductivity 1.15 W/m-K

@Temperature 100 °C
7.98 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast A Vuurvast Dense Refractory Brick
Description: A general purpose high quality fireclay brick for use up to 1400°C. Reasonably good thermal shock resistance.Remarks: This data represents average values, obtained from samples that ..
Thermal Conductivity 1.15 - 1.35 W/m-K

@Temperature 100 °C
7.98 - 9.37 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast FLUCON 160 H SiC (R) Dense Self Flowing Refractory Castable
Description: Flucon 160 H SiC (R) is a self-flowing low cement castable, characterized by a high strength and good slag resistance. Because of the presence of SiC this material has a very good resis..
Thermal Conductivity 1.15 - 1.35 W/m-K

@Temperature 100 °C
7.98 - 9.37 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast FLUCON 160 H Dense Self Flowing Refractory Castable
Description: Flucon 160 H is a self-flowing low cement castable on high fired high alumina grog base, characterized by a high strength and good thermal shock resistance.Remarks: These values apply t..