Material Notes:
Description: A general purpose high quality fireclay brick for use up to 1400°C. Reasonably good thermal shock resistance.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 2.15 g/cc
0.0777 lb/in³
Apparent
Porosity <= 20 %
<= 20 %
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 35.0 MPa
5080 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.15 W/m-K

@Temperature 100 °C
7.98 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.25 W/m-K

@Temperature 650 °C
8.68 BTU-in/hr-ft²-°F

@Temperature 1200 °F
1.38 W/m-K

@Temperature 1100 °C
9.58 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Maximum Service Temperature, Air 1400 °C
2550 °F
1450 °C
2640 °F
Deformation under load - t<sub>a</sub>
Component Elements Properties Metric English Comments
Al2O3 40 %
40 %
Fe2O3 <= 2.0 %
<= 2.0 %
SiO2 53 %
53 %
Descriptive Properties Value Comments
Segercone 34
Thermal Shock Resistance 15 cycles
DIN 51068