Thermal Properties Metric English Comments
Thermal Conductivity 99.20 W/m-K

@Temperature 200 °C
688.4 BTU-in/hr-ft²-°F

@Temperature 392 °F
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T6
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Thermal Conductivity 99.20 W/m-K

@Temperature 300 °C
688.4 BTU-in/hr-ft²-°F

@Temperature 572 °F
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T6
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Thermal Conductivity 99.20 W/m-K

@Temperature 200 °C
688.4 BTU-in/hr-ft²-°F

@Temperature 392 °F
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Thermal Conductivity 99.20 W/m-K

@Temperature 300 °C
688.4 BTU-in/hr-ft²-°F

@Temperature 572 °F
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Thermal Conductivity 99.20 W/m-K

@Temperature 300 °C
688.4 BTU-in/hr-ft²-°F

@Temperature 572 °F
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T4
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Thermal Conductivity 99.20 W/m-K

@Temperature 200 °C
688.4 BTU-in/hr-ft²-°F

@Temperature 392 °F
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T4
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..