Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.580 - 0.680 W/m-K @Temperature 600 °C |
4.03 - 4.72 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 127 S GM Dense Refractory Castable Description: Curon 127 S GM gunning castable is characterized by a reasonable strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks:.. |
|||
Thermal Conductivity | 0.580 - 0.680 W/m-K @Temperature 600 °C |
4.03 - 4.72 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 145 CC Dense Refractory Castable Description: This castable is especially developed for strong, large constructions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.580 - 0.680 W/m-K @Temperature 600 °C |
4.03 - 4.72 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 150 H Dense Refractory Castable Description: Curon 150 H is composed of a very pure grog combined with a high quality high alumina cement. It is characterized by a good resistance against thermal shock and against reducing operati.. |
|||
Thermal Conductivity | 0.582 W/m-K @Temperature 260 °C |
4.03 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Chosun Refractories HACT-150 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |