Gouda Vuurvast CURON 150 H Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 150 H Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Curon 150 H is composed of a very pure grog combined with a high quality high alumina cement. It is characterized by a good resistance against thermal shock and against reducing operating conditions.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.10 - 2.20 g/cc
0.0759 - 0.0795 lb/in³
After drying at 110°C
Particle Size <= 7000 µm
<= 7000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 25.0 - 35.0 MPa

@Temperature 1300 °C
3630 - 5080 psi

@Temperature 2370 °F
Cold Crushing Strength
40.0 - 50.0 MPa

@Temperature 100 °C
5800 - 7250 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.530 - 0.630 W/m-K

@Temperature 100 °C
3.68 - 4.37 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.580 - 0.680 W/m-K

@Temperature 600 °C
4.03 - 4.72 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.660 - 0.760 W/m-K

@Temperature 1300 °C
4.58 - 5.27 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1500 °C
2730 °F
Shrinkage -0.500 - 0.500 %

@Temperature 1300 °C
-0.500 - 0.500 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 48 %
48 %
Fe2O3 <= 2.0 %
<= 2.0 %
SiO2 44 %
44 %
Descriptive Properties Value Comments
ASTM Classification D
Material Consumption per 1 m3 2050 kg
Mixing Water 11-13 liters
per 100 kgs dry material