Thermal Properties Metric English Comments
Thermal Conductivity 26.7 W/m-K

@Temperature 900 °C
185 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes Hastelloy® X alloy, sheet
Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ..
Thermal Conductivity 26.7 W/m-K

@Temperature 1090 °C
185 BTU-in/hr-ft²-°F

@Temperature 2000 °F
ATI Allvac® 718Plus™ Nickel Superalloy
Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the..
Thermal Conductivity 26.7 W/m-K

@Temperature 343 °C
185 BTU-in/hr-ft²-°F

@Temperature 650 °F
Schmolz + Bickenbach Cryodur® 2363 (A-2) Cold Work Die Steel
Description: Cryodur® 2363 is a cold-work steel developed for an excellent combination of wear resistance and toughness and Supplied in the annealed conditionCharacteristics: Good wear resistance; ..
Thermal Conductivity 26.7 W/m-K

@Temperature 21.1 °C
185 BTU-in/hr-ft²-°F

@Temperature 70.0 °F
Schmolz + Bickenbach Thermodur® 2343 EFS Extra Fine Structure (H-11)- Hot Work Die Steel
Description: Thermodur® 2343 is a single melt Extra Fine Structure (EFS) hot work die steel and Supplied in the annealed conditionCharacteristics: Good toughness; Moderate high-temperature strength..