Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 250 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 36.0 W/m-K

@Temperature 20.0 °C
250 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Latrobe LSSâ„¢ 2714 Hot Work Tool Steel (DIN 1.2714 mod)
TLS 2714 is a nickel-chromium-molybdenum hot work steel that exhibits high impact toughness and good resistance to softening at elevated temperature. The high nickel content imparts the toughness as..
Thermal Conductivity 36.0 W/m-K

@Temperature 20.0 °C
250 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Latrobe LSSâ„¢ 2714T Hot Work Tool Steel (DIN 1.2714 mod)
TLS 2714HT is the same steel available from inventory in a heat-treated condition, at a hardness of 352 to 401 HBS (approximately 38 to 43 HRC). TLS 2714HT can be readily flame cut, and this propert..
Thermal Conductivity 36.0 W/m-K

@Temperature 20.0 °C
250 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Zircar Ceramics Alumina Furnaceware
ZIRCAR Ceramics Alumina Furnaceware are high purity fully dense, fine grain aluminum oxide products suitable for use in applications with temperatures as high as 1800°C. Such uses include crucibles..
Thermal Conductivity 36.0 W/m-K

@Temperature 20.0 °C
250 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
hardness of 40 HRC
Bohler-Uddeholm UDDEHOLM ALVAR 14 Hot Work Tool Steel
Alvar 14 is a chromium-nickel-molybdenumvanadium alloyed steel ALVAR 14 is characterized by: Good toughnessGood resistance to high thermal stresses Good stability in hardeningGood through-hardening..
Thermal Conductivity 36.0 W/m-K

@Temperature 100 °C
250 BTU-in/hr-ft²-°F

@Temperature 212 °F
ATI Allegheny Ludlum AL 304DA Stainless/Carbon Steel Three-Ply Composite
Composition above represents only the Type 304 cladding. Its iron content calculated as balance.Allegheny Ludlum AL 304DA is tri-ply composite consisting of a dual stabilized, low carbon steel cent..