Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 25.0 W/m-K @Temperature <=200 °C |
174 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP1 H13 3/4 hard, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature <=200 °C |
174 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP1C H12 1/2 hard, Rolled Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature <=200 °C |
174 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP1 H11 1/4 hard, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature <=200 °C |
174 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP1 H11 1/4 hard, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature <=200 °C |
174 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP1 H13 3/4 hard, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature <=200 °C |
174 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP1 H14 4/4 hard, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature <=200 °C |
174 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP1C H11 1/4 hard, Rolled Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature <=200 °C |
174 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP1C H15 Spring, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature <=200 °C |
174 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP1D H14 4/4 hard, Drawn Copper Alloy, Wire and rod, 2.5< diameter< 5 High Corrosion Resistance: ARCAP alloys are very corrosion resistant to the majority of chemical and physical environments. CLAL can provide data for the corrosion resistance of ARCAP alloys. In par.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature <=200 °C |
174 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP1D H14 4/4 hard, Drawn Copper Alloy, Wire and rod, 5 High Corrosion Resistance: ARCAP alloys are very corrosion resistant to the majority of chemical and physical environments. CLAL can provide data for the corrosion resistance of ARCAP alloys. In par.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature <=200 °C |
174 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP1D H14 4/4 hard, Drawn Copper Alloy, Wire and rod, diameter High Corrosion Resistance: ARCAP alloys are very corrosion resistant to the majority of chemical and physical environments. CLAL can provide data for the corrosion resistance of ARCAP alloys. In par.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 20.0 °C |
174 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Bohler-Uddeholm BÖHLER M261 Extra Plastic Lens Mold Steel VACUUM ARC REMELTED HARDENED AND TEMPERED PLASTIC LENS MOLD STEELBOHLER M261 follow current trends in tool and die-making:Excellent machinability coupled with higher hardnessGood dimensional stabili.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 20.0 °C |
174 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 600.0 °C |
174 BTU-in/hr-ft²-°F @Temperature 1112 °F |
hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 30 AISI M2 + Co SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel Uddeholm Vanadis 30 is a Co high alloyed powder metallurgy high speed steel corresponding to AISI M3:2 + Co. The high compressive strength, 67 HRC, and good abrasive wear resistance makes Uddeholm V.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 399 °C |
174 BTU-in/hr-ft²-°F @Temperature 750 °F |
hardness of 60 HRC |
Bohler-Uddeholm UDDEHOLM VANADIS 6 Cold Work Tool Steel Description: Chromium-molybdenum-vanadium alloyed PM steel. Toolmaking with highly alloyed tool steel means that machining and heat treatment have to be considered more than with lower alloyed grade.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 399 °C |
174 BTU-in/hr-ft²-°F @Temperature 750 °F |
hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W .. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 400 °C |
174 BTU-in/hr-ft²-°F @Temperature 752 °F |
hardened and tempered condition |
Assab Steels ASP 60 Cold Work Steel ASP 60 is a W-Mo-V-Co alloyed PM high speed steel characterized by:Highest wear resistanceMaximum compressive strengthGood through hardening propertiesGood toughnessGood dimensional stability on hea.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 400 °C |
174 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Assab Steels ASSAB 88 Cold Work Steel ASSAB 88 (SLEIPNER) is a chromium-molybdenum-vanadium alloyed tool steel which is characterized by:Good wear resistanceGood chipping resistanceHigh compressive strengthHigh hardness (>60HRC) after h.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 100 °C |
174 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.Information provided by Allegheny Ludlum |