Thermal Properties Metric English Comments
Thermal Conductivity 20.9 W/m-K

@Temperature 600 °C
145 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® X alloy, sheet
Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ..
Thermal Conductivity 20.9 W/m-K

@Temperature 700 °C
145 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Haynes Waspaloyâ„¢ alloy, sheet
Age-hardenable superalloy with very good strength at temperatures up 980°C (1800°F), can be cold-formed in the annealed condition, may also be hot formed at 1040°C (1900°F) and above, go..
Thermal Conductivity 20.9 W/m-K

@Temperature 95.0 °C
145 BTU-in/hr-ft²-°F

@Temperature 203 °F
Crucible Steel AIRDI® 150 (AISI D2) Tool Steel
Airdi 150 (AISI D2) is an air-hardening, high carbon, high chromium tool steel, heat treatable to HRC 60-62. It offers excellent abrasion resistance, due to a large volume of carbides in the microst..