Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, mill annealed HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GMAW spray weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld 3.2 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, 25.4 mm thick bar HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet, GTAW weld HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, 30% cold rolled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, 50% cold rolled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 1 hour at 500°C, air cooled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, 6.4 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, 9.5 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, all-weld metal, GMAW weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 600 °C |
130 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
HP Alloys Alloy B-2, Solution Treated, 10% Cold Worked Solution Treated, 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 600 °C |
130 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
HP Alloys Alloy B-2, Solution Treated, 20% Cold Worked Solution Treated, 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 600 °C |
130 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
HP Alloys Alloy B-2, Solution Treated, 30% Cold Worked Solution Treated, 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 600 °C |
130 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 600 °C |
130 BTU-in/hr-ft²-°F @Temperature 1110 °F |
Annealed Condition |
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 20.0 - 500 °C |
130 BTU-in/hr-ft²-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum 309 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 20.0 - 500 °C |
130 BTU-in/hr-ft²-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum 309H Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 20.0 - 500 °C |
130 BTU-in/hr-ft²-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum 309Si Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 20.0 - 500 °C |
130 BTU-in/hr-ft²-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum 310 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 20.0 - 500 °C |
130 BTU-in/hr-ft²-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum 310S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 20.0 - 500 °C |
130 BTU-in/hr-ft²-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum 310Si Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, 0.71 mm thick sheet HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, 10% cold rolled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW short arc weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, 19.1 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, 31.8 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 600 °C |
130 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Thermal Conductivity | 18.7 W/m-K @Temperature 400 °C |
130 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |