Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.60 - 1.80 W/m-K @Temperature 110 °C |
11.1 - 12.5 BTU-in/hr-ft²-°F @Temperature 230 °F |
|
Gouda Vuurvast FLUCON 150 G (R) Dense Self Flowing Refractory Castable Description: Flucon 150 G (R) is a self-flowing low cement castable based on sintered South-American bauxite. Especially suitable for direct contact with liquid aluminum metal.Remarks: These values .. |