Polymer Property : Thermal Conductivity = 1.80 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.60 - 1.80 W/m-K

@Temperature 110 °C
11.1 - 12.5 BTU-in/hr-ft²-°F

@Temperature 230 °F
Gouda Vuurvast FLUCON 150 G (R) Dense Self Flowing Refractory Castable
Description: Flucon 150 G (R) is a self-flowing low cement castable based on sintered South-American bauxite. Especially suitable for direct contact with liquid aluminum metal.Remarks: These values ..