Material Notes:
Description: Because this material contains a high percentage of sillimanite, it has a very good thermal shock resistance together with a very good slag resistance. Therefore this material finds its application in heavily treated burner throats.Remarks: The stated chemical composition and physical properties represent average values.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.20 - 2.30 g/cc
0.0795 - 0.0831 lb/in³
After drying at 110°C
Thermal Properties Metric English Comments
Thermal Conductivity 0.900 - 1.10 W/m-K

@Temperature 100 °C
6.25 - 7.63 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.10 - 1.30 W/m-K

@Temperature 600 °C
7.63 - 9.02 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.22 - 1.42 W/m-K

@Temperature 1100 °C
8.47 - 9.85 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Shrinkage -1.60 - 1.60 %

@Temperature 1100 °C
-1.60 - 1.60 %

@Temperature 2010 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 60 %
60 %
Fe2O3 0.90 %
0.90 %
SiO2 35 %
35 %
Descriptive Properties Value Comments
Bonding Type chemical/ceramic
Material Consumption per 1 m3 2400 kg
Segercone 35
Workability 20-25%
ASTM C181-176