Polymer Property : Thermal Conductivity = 1.28 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.28 - 1.48 W/m-K

@Temperature 600 °C
8.88 - 10.3 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 180 B Dense Refractory Castable
Description: This high quality castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of Fe2O3, this castable can..
Thermal Conductivity 1.28 - 1.48 W/m-K

@Temperature 600 °C
8.88 - 10.3 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 180 Dense Refractory Castable
Description: This high quality, corundum based castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of SiO2, th..
Thermal Conductivity 1.28 - 1.48 W/m-K

@Temperature 600 °C
8.88 - 10.3 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 180 TF Dense Refractory Castable
Description: Curon 180 TF is a tabular alumina based castable, highly abrasion resistant, especially developed for application in the vacuum ladle treatment installation in the steel refinery.Remark..
Thermal Conductivity 1.28 - 1.38 W/m-K

@Temperature 600 °C
8.88 - 9.58 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast VIBRON 170 M Dense Vibrating Refractory Castable
Description: Vibron 170 is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid slags.Remar..
Thermal Conductivity 1.28 - 1.38 W/m-K

@Temperature 600 °C
8.88 - 9.58 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast VIBRON 170 M GS (R) Dense Vibrating Refractory Castable
Description: Vibron 170 M GS (R) is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sl..
Thermal Conductivity 1.28 - 1.38 W/m-K

@Temperature 600 °C
8.88 - 9.58 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast VIBRON 170 M RAPID Dense Vibrating Refractory Castable
Description: Vibron 170 M Rapid is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sla..
Thermal Conductivity 1.28 W/m-K

@Temperature 600 °C,
Time 10800 sec
8.88 BTU-in/hr-ft²-°F

@Temperature 1110 °F,
Time 3.00 hour
Sharadaa Ceramics REFCAST 80 High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Thermal Conductivity 1.28 W/m-K

@Temperature 400 °C,
Time 10800 sec
8.88 BTU-in/hr-ft²-°F

@Temperature 752 °F,
Time 3.00 hour
Sharadaa Ceramics REFCAST A High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Thermal Conductivity 1.28 W/m-K

@Temperature 600 °C,
Time 10800 sec
8.88 BTU-in/hr-ft²-°F

@Temperature 1110 °F,
Time 3.00 hour
Sharadaa Ceramics REFCAST LC60 Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Thermal Conductivity 1.28 W/m-K

@Temperature 800 °C,
Time 10800 sec
8.88 BTU-in/hr-ft²-°F

@Temperature 1470 °F,
Time 3.00 hour
Sharadaa Ceramics REFCAST LC60ABR Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Thermal Conductivity 1.28 - 1.48 W/m-K

@Temperature 600 °C
8.88 - 10.3 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 180 T Sp Dense Refractory Castable
Description: Curon 180 T special is a tabular alumina based castable, highly resistant against abrasion, dust erosion or heavy impact even at extremely high temperatures.Remarks: These values apply ..
Thermal Conductivity 1.28 - 1.48 W/m-K

@Temperature 1600 °C
8.88 - 10.3 BTU-in/hr-ft²-°F

@Temperature 2910 °F
Gouda Vuurvast CURON 185 T Dense Refractory Castable
Description: Curon 185 T is a very pure high alumina castable based on tabular alumina with very low Fe2O3 and SiO2 contents. Suitable for use in strongly reducing atmospheres.Remarks: These values ..