Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.270 W/m-K @Temperature 400 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Pyrotek B-3A REFRACTORY BOARD Pyrotek B-3A is a high density calcium silicate board specifically designed for demanding applications such as holding furnaces, launder linings and baffle plates. Its high density and superior har.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 600 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Pyrotek B-3A REFRACTORY BOARD Pyrotek B-3A is a high density calcium silicate board specifically designed for demanding applications such as holding furnaces, launder linings and baffle plates. Its high density and superior har.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 1650 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 3000 °F |
|
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 250 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 482 °F |
ASTM E1530 |
3M Dyneon™ CC174-N PTFE, 15% Fiberglass/Moly Filled
(discontinued **) Product Form: Gray, non-pelletized powder. Applications include bearings, rider rings, and packings.Data provided by Dyneon. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 250 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 482 °F |
ASTM E1530 |
3M Dyneon™ TF 4103 PTFE 15% Glass Fiber Filled
(discontinued **) Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon. |
|||
Thermal Conductivity | 0.270 - 0.370 W/m-K @Temperature 200 °C |
1.87 - 2.57 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Gouda Vuurvast GI 28 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.270 - 0.350 W/m-K @Temperature 600 °C |
1.87 - 2.43 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GOLITE 1.2.4. MIX GM Refractory Insulating Castable Description: This light weight gunning castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Re.. |
|||
Thermal Conductivity | 0.270 - 0.370 W/m-K @Temperature 1000 °C |
1.87 - 2.57 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast GOLITE 125 R GM Refractory Insulating Castable Description: Golite 125 R GM has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products.Informati.. |
|||
Thermal Conductivity | 0.270 - 0.370 W/m-K @Temperature 1260 °C |
1.87 - 2.57 BTU-in/hr-ft²-°F @Temperature 2300 °F |
|
Gouda Vuurvast GOLITE 135 L Refractory Insulating Castable Description: Golite 135 L can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning va.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 600 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-201 supplemented by ASTM C-182 |
Skamol Group SKAMOCAST 14-105 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 600 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-201 supplemented by ASTM C-182 |
Skamol Group VERMICAST 14-100 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 816 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 1500 °F |
6 pcf |
Thermal Ceramics Cerablanket Blanket Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on ave.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 816 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 1500 °F |
6 pcf |
Thermal Ceramics Cerachem Blanket Cerachem Blanket is a 2600°F (1427°C) maximum temperature rated refractory blanket formed from a unique, patented, spun alumina-silica-zirconia fiber. It is specially designed for applications whe.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 816 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 1500 °F |
6 pcf |
Thermal Ceramics Cerachrome Blanket Made from spun alumina-silica-chromia fiber, Cerachrome Blanket is well suited for hot face lining applications where higher temperatures are encountered, such as soaking pit covers, reheat and forg.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 816 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 1500 °F |
6 pcf |
Thermal Ceramics Kaowool S Blanket Kaowool S Blanket is produced from high quality spun fibers. It is available in a wide variety of densities and sizes, and offers a highly cost effective alternative to Cerablanket with its 2300°F .. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 1650 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 3000 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics AL-25/1700 Alumina Insulation AL-25/1700 is a rigid medium duty grade of alumina fiber board. Not as strong as SALI but capable of delivering years of service.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 1650 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 3000 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics AL-30 Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 1650 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 3000 °F |
parallel to thickness; ASTM C177-76 |
Zircar Ceramics AL-30AAH Alumina Insulation AL-30AAH was developed for use in copper vapor lasers where the ultimate in low mass alumina purity is required.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 427 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 801 °F |
|
Zircar Refractory Composites RS-99-60 Refractory Sheet ZRCI Refractory Sheet Type RS-99-60 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 400 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 752 °F |
parallel to thickness |
Zircar Refractory Composites ZIRCAL-95 Refractory Board Type ZIRCAL-95 Refractory Board is produced from a combination of natural organic fibers and inert reinforcing fillers in a high density calcium silicate hydrate matrix. Designed as a substitute for.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 1650 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 3000 °F |
|
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 1650 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 3000 °F |
|
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 260 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 500 °F |
ASTM C182 |
BNZ Materials BNZ-26 HS Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 538 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 1000 °F |
ASTM C182 |
BNZ Materials BNZ-26 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 800 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 1470 °F |
ASTM C182 |
BNZ Materials BNZP-23B Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 800 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 1470 °F |
ASTM C182 |
BNZ Materials BNZP-25L Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 400 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTM C182 |
BNZ Materials Color B Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 1650 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 3000 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics AL-30AA Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 1100 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 2010 °F |
parallel to thickness |
Zircar Ceramics ASQ Castertip 14 pcf density refractory ceramic fiber "soft tip". Alumina bonding of shot free fiber results in extreme performance in manufacture of the finest grades of medical, food and packaging foils. Inform.. |
|||
Thermal Conductivity | 0.270 W/m-K @Temperature 1650 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 3000 °F |
|
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |