Maximum Service Temperature, Air 97.8 °C
208 °F
Heat Distortion, Annealed; ASTM D648
Total 819E Polystyrene  (discontinued **)
Polystyrene 819E is a high impact polystyrene extrusion grade with very high stiffness and thermal properties.It makes an excellent gloss/cut resistant layer for foam applications or general thermof..
Maximum Service Temperature, Air 97.8 °C
208 °F
Heat Distortion, Annealed; ASTM D648
Total 965E Polystyrene  (discontinued **)
Polystyrene 965E is a high-impact polystyrene. The extruder will see that 965E produces sheet with a dull matte finish and superior wetting tension to meet the printers needs.965E is specially desig..