Total 819E Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total 819E Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polystyrene 819E is a high impact polystyrene extrusion grade with very high stiffness and thermal properties.It makes an excellent gloss/cut resistant layer for foam applications or general thermoforming applications where high temperature resistance is required.Information provided by Total Petrochemicals, Inc.
Physical Properties Metric English Comments
Melt Flow 2.6 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.6 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D638
Elongation at Yield 55 %
55 %
ASTM D638
Tensile Modulus 2.28 GPa
330 ksi
ASTM D638
Flexural Strength 62.1 MPa
9000 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm
2.20 ft-lb/in
ASTM D256
Falling Dart Impact 14.68 J
10.83 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 97.8 °C
208 °F
Heat Distortion, Annealed; ASTM D648
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Optical Properties Metric English Comments
Gloss 85 %
85 %
60°; ASTM D523