Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
ND Industries 907 Anti-seize Aluminum-Graphite Aluminum and Graphite based, general purpose lubricant |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
Lucas-Milhaupt Dry Flux Silver Brazing Flux Dry Flux is a premium quality brazing flux in powdered form consisting of a unique combination of borates and fluorides for use with torch, induction, furnace, resistance, dip and other heating meth.. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
Lucas-Milhaupt Ultra Flux Silver Brazing Flux Ultra Flux is a water base paste consisting of a unique combination of potassium salts of fluorine and boric acid. It is recommended for use with torch, induction, furnace, resistance, dip and other.. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | long continuous heating |
Meehanite HSV Heat Resisting Cast Iron Type HSV is an iron developed essentially for engineering parts subjected to long continuous heating. It has been designed to have the maximum load bearing ability.General Meehanite information - M.. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
Lucas-Milhaupt Dispensable Flux Dispensable Flux is a water base consisting of a unique combination of potassium salts of fluorine and boric acid. It is recommended for use with torch, induction, furnace, resistance, dip and other.. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
Universal Wire Works 347 Stainless Steel Electrode Universal 347 electrodes were developed for the welding of types 321 and 347 stainless and the clad side of steel clad with like alloys. Alloy 347 is used for the fabrication of equipment, which mus.. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
Universal Wire Works 430 Stainless Steel Electrode Universal 430 electrode deposits contain approximately 16% chromium in a carefully balanced composition to provide outstanding resistance at temperatures up to 1600 degrees F. Deposits are martensit.. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
XADC-Armoloy Armoloy® TDC Hard Chromium Coating ARMOLOY® TDC is a low temperature, multi-state surface finishing process. ARMOLOY® utilizes proprietary chemical solutions and application processes that are carefully monitored to produce it.. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
BNZ Materials 460 Insulating Cement 460 Insulating Cement is a 1600°F product, provided in higher density than 508 Insulating Cement. 460 Cement can be applied in heavy layers. It is frequently used as the principal covering on pipe .. |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | |
Aremco Pyro-Putty™ 2500 High Temperature Ceramic-Metallic Putty, Iron Oxide Filled Ceramic and Black Iron Oxide-Filled, One-Part, Water Based Paste.For Applications to 1/4" Thick.Repairs Cast Iron, and Steel Parts to 1600°F |
|||
Maximum Service Temperature, Air | 871 °C | 1600 °F | Continuous |
Aremco Quartz-Coat™ 850 High Temperature Specialty Coatings Inorganic, Glass-Ceramic Filled Glass-ceramic, white reflective coating for glass and quartz to 1500°F (816°F) |