Universal Wire Works 430 Stainless Steel Electrode

Category Metal , Ferrous Metal , Stainless Steel , T 400 Series Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 430 Stainless Steel Electrode.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universal 430 electrode deposits contain approximately 16% chromium in a carefully balanced composition to provide outstanding resistance at temperatures up to 1600 degrees F. Deposits are martensitic in structure requiring preheat and postweld heat treatment. Optimum physical and corrosion properties are obtained when the proper heat treat operation is done after welding.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 538 MPa
78000 psi
Elongation at Break 28 %
28 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 871 °C
1600 °F
Component Elements Properties Metric English Comments
Carbon, C 0.070 %
0.070 %
Chromium, Cr 16.6 %
16.6 %
Iron, Fe 81.7 %
81.7 %
As Remainder
Manganese, Mn 0.95 %
0.95 %
Silicon, Si 0.64 %
0.64 %