Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 87.8 °C | 190 °F | Heat Distortion, Annealed; ASTM D648 |
Total 620 Polystyrene
(discontinued **) Polystyrene 620 is an impact polystyrene designed for high gloss cap layers. The polymer has been specifically designed for co extrusion processing to produce a ductile sheet with an extremely high .. |
|||
Maximum Service Temperature, Air | 87.8 °C | 190 °F | |
Garlock 2264 C.I. EPDM Sheet Rubber, Polyester Insert Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2564 is a smooth fini.. |
|||
Maximum Service Temperature, Air | 87.8 °C @Pressure <=1.03 MPa |
190 °F @Pressure <=150 psi |
|
Garlock 244 Neoprene Rubber - Commercial Grade Soft blend of neoprene, nitrile and SBR rubbers for use as bumpers, pads, and in sealing and general gasket applications. It is not recommended in applications where high oil resistance is required.. |
|||
Maximum Service Temperature, Air | 87.8 °C | 190 °F | |
Sika Industry SikaFlex 221 Fast Cure Polyurethane Sealant/Adhesive Sika 221 SikaFlex Fast Cure Polyurethane Sealant/AdhesiveThis versatile product is the most popular adhesive/sealant. It is an excellent adhesive/sealant and can handle many light bonding applicatio.. |
|||
Maximum Service Temperature, Air | 87.8 °C | 190 °F | |
Sika Industry SikaFlex 201 Adhesive Sika 201 SikaFlex AdhesiveSikaflex 201 meets Federal Specification TT-S-00230C, Type II, Class A and ASTK C-920, Type S, Grade NS. 15 - 15 mm Cut-Off. Good non-sag. Available in black, white, gray, .. |
|||
Maximum Service Temperature, Air | 87.8 °C | 190 °F | |
Master Bond MB514 Hot Melt Adhesive Compound Master Bond Hot Melt MB514 is a high performance hot melt adhesive with the following key features: It is particularly suited for use on untreated surfaces of high and low density polyethylene, poly.. |
|||
Maximum Service Temperature, Air | 87.8 °C | 190 °F | Heat Distortion, Annealed; ASTM D648 |
Total PSI 625 Polystyrene Polystyrene 625 is a medium impact polystyrene with balanced physical properties. Thin walled parts with complex runners and gates, run fast and consistently with the easy flow 625. The natural whi.. |