Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 88.0 °C | 190 °F | Maximum operating temperature continuously for 5000 hours based on a tensile stress of 50% at 23° C. (dry sample) |
Omnia Plastica Omniamid PA 6 - Akulon 6 - at 50% RH Semi-crystalline polymer of polyamide obtained by the polymerisation of the caprolactam. Its large popularity is due to both its good overall features as well as its cost-performance relationship. T.. |
|||
Maximum Service Temperature, Air | 88.0 °C | 190 °F | Maximum operating temperature continuously for 5000 hours based on a tensile stress of 50% at 23° C. |
Omnia Plastica Omniamid PA 6 - Akulon 6 - Dry Semi-crystalline polymer of polyamide obtained by the polymerisation of the caprolactam. Its large popularity is due to both its good overall features as well as its cost-performance relationship. T.. |
|||
Maximum Service Temperature, Air | 87.8 °C | 190 °F | Heat Distortion, Annealed; ASTM D648 |
Total 620 Polystyrene
(discontinued **) Polystyrene 620 is an impact polystyrene designed for high gloss cap layers. The polymer has been specifically designed for co extrusion processing to produce a ductile sheet with an extremely high .. |
|||
Maximum Service Temperature, Air | 88.0 - 204 °C | 190 - 399 °F | Average value: 136 °C Grade Count:10 |
Overview of materials for Silicone, RTV, Construction Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Construction Grade". Each property range of values reported is minimum and maximum values.. |
|||
Maximum Service Temperature, Air | 87.8 °C | 190 °F | |
Garlock 2264 C.I. EPDM Sheet Rubber, Polyester Insert Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2564 is a smooth fini.. |
|||
Maximum Service Temperature, Air | 87.8 °C @Pressure <=1.03 MPa |
190 °F @Pressure <=150 psi |
|
Garlock 244 Neoprene Rubber - Commercial Grade Soft blend of neoprene, nitrile and SBR rubbers for use as bumpers, pads, and in sealing and general gasket applications. It is not recommended in applications where high oil resistance is required.. |
|||
Maximum Service Temperature, Air | 88.0 °C | 190 °F | Elasticity is retained to this temperature. |
Momentive Performance Materials Ultraglaze® 4000 Construction Sealant High strength, one-part structural glazing/weathersealing system. Cure Method: Alkoxy (Neutral). Tack-free time 2 to 5 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Sili.. |
|||
Maximum Service Temperature, Air | 88.0 °C | 190 °F | Elasticity is retained to this temperature. |
Momentive Performance Materials Ultraglaze® SSG 4000AC Construction Sealant High strength, one-part, accelerated-cure structural glazing/weathersealing system.Cure Method: Alkoxy (Neutral). Tack-free time 1 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silico.. |
|||
Maximum Service Temperature, Air | 88.0 °C | 190 °F | Heat Distortion Temp |
Hannam Chemical Hanalac 770 ABS, Extrusion Grade FDA Approved. Excellent mechanical strength, high rigidity, and high impact strength. Good thermoformability. Applications: Refrigerators liners, bathtubs, automobile interiors, portable bags, n.. |
|||
Maximum Service Temperature, Air | 88.0 °C | 190 °F | Heat Distortion Temp |
Hannam Chemical Hanalac 775 ABS, Extrusion Grade Increased chemical resistance. Excellent mechanical strength, high rigidity, and high impact strength. Good thermoformability. Applications: Refrigerators liners, bathtubs, automobile interiors,.. |
|||
Maximum Service Temperature, Air | 87.8 °C | 190 °F | |
Sika Industry SikaFlex 221 Fast Cure Polyurethane Sealant/Adhesive Sika 221 SikaFlex Fast Cure Polyurethane Sealant/AdhesiveThis versatile product is the most popular adhesive/sealant. It is an excellent adhesive/sealant and can handle many light bonding applicatio.. |
|||
Maximum Service Temperature, Air | 87.8 °C | 190 °F | |
Sika Industry SikaFlex 201 Adhesive Sika 201 SikaFlex AdhesiveSikaflex 201 meets Federal Specification TT-S-00230C, Type II, Class A and ASTK C-920, Type S, Grade NS. 15 - 15 mm Cut-Off. Good non-sag. Available in black, white, gray, .. |
|||
Maximum Service Temperature, Air | 87.8 °C | 190 °F | |
Master Bond MB514 Hot Melt Adhesive Compound Master Bond Hot Melt MB514 is a high performance hot melt adhesive with the following key features: It is particularly suited for use on untreated surfaces of high and low density polyethylene, poly.. |
|||
Maximum Service Temperature, Air | 87.8 °C | 190 °F | Heat Distortion, Annealed; ASTM D648 |
Total PSI 625 Polystyrene Polystyrene 625 is a medium impact polystyrene with balanced physical properties. Thin walled parts with complex runners and gates, run fast and consistently with the easy flow 625. The natural whi.. |
|||
Maximum Service Temperature, Air | 88.0 °C | 190 °F | |
3M 4200 Marine Adhesive/Sealant Fast Cure A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds to wood, gelcoat and fiberglass. It forms watertight, weather-resistant seals on joints an.. |
|||
Maximum Service Temperature, Air | 88.0 °C | 190 °F | |
3M 5200 Marine Adhesive/Sealant 3M™ Marine Adhesive/Sealant 5200 is a one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds. It has excellent adhesion to wood, gelcoat and fiberglass. It for.. |
|||
Maximum Service Temperature, Air | 88.0 °C | 190 °F | |
3M 5200 Marine Adhesive/Sealant Fast Cure A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds with excellent adhesion to wood and fiberglass. Forms watertight, weather-resistant seals .. |
|||
Maximum Service Temperature, Air | 88.0 °C | 190 °F | Elasticity is retained to this temperature. |
Momentive Performance Materials Ultraglaze® 4400 Construction Sealant High strength, two-part structural glazing system. Cure Method: Condensation. Tack-free time 3 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of .. |