Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 815 °C | 1500 °F | |
Pyrotek A-5C Fiberglass Fabric Z-5 with proprietary Pyroseal red coating on one side to provide an airtight covering while maintaining flexibility.Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 815 °C | 1500 °F | |
Pyrotek Z-5 Fiberglass Fabric Fiberglass, coarse textile fiber. Woven fabric.Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 815 °C | 1500 °F | |
Pyrotek Z-6W Fabric Wire reinforced, this material is good for any area requiring an abrasion-resistant material.Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 815 °C | 1500 °F | |
Tritex TRI-F Blanket Insulation TRI-F is a unique thermal and acoustic insulation that combines three high temperature fibers in a patented process. The result is a blanket with a service life to 1500°F. By blending fibers of var.. |