Wire reinforced, this material is good for any area requiring an abrasion-resistant material.Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.589 g/cc
0.0213 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 815 °C
1500 °F