Material Notes:
Closed-cell polyethylene foam. Extruded reticulated pieces. Excellent physical properties both for active and static uses. Adjustable softness, elasticity, thermal deformation, shock absorbing. Used as thermal insulation. Feastures minimal water absorption, low water-vapour permeability, resistance to atmospheric agents, non-polluting, chemically inert.Information provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.0200 - 0.0400 g/cc
0.000723 - 0.00145 lb/in³
ISO 845-88
Water Absorption <= 5.0 %
<= 5.0 %
ASTM D 1056
Mechanical Properties Metric English Comments
Hardness, Shore OO 45 - 55
45 - 55
ASTM D 2240
Tensile Strength 0.200 MPa
29.0 psi
ASTM D 412
Elongation at Break >= 200 %
>= 200 %
ASTM D 412
Tear Strength 0.120 kN/m
0.685 pli
ASTM D 624
Compression Set 15 %

@Strain 25.0 %
15 %

@Strain 25.0 %
ASTM D 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 °C
158 °F
ASTM D 3575
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
ASTM D 3575
Shrinkage <= 5.0 %

@Temperature 70.0 °C,
Time 605000 sec
<= 5.0 %

@Temperature 158 °F,
Time 168 hour
Linear; ASTM D 1204
Descriptive Properties Value Comments
Cellular Structure Closed
Color Grey, White
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC