Polymer Property : Maximum Service Temperature, Air = 85.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 - 85.0 °C
158 - 185 °F
ISO.75 DN.53461
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300
PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom..
Maximum Service Temperature, Air 70.0 - 85.0 °C
158 - 185 °F
ISO.75 DN.53461
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300
PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom..
Maximum Service Temperature, Air 60.0 - 85.0 °C
140 - 185 °F
Average value: 66.3 °C Grade Count:4
Overview of materials for PVC, Uncompounded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate ..
Maximum Service Temperature, Air 75.0 - 85.0 °C
167 - 185 °F
Softening Range
Huntsman Araldite GT 7072 US Bisphenol A Epoxy Solid Resin
Weight per Epoxide (EEW, g/eq) 600 to 700. Max color is 1.Comments/Applications: Unmodified bis A "Type 2" epoxy. Used in trade sales paint, concrete, maintenance and powder coatings as a modifier..
Maximum Service Temperature, Air 75.0 - 85.0 °C
167 - 185 °F
Softening Range
Huntsman Araldite GT 9654 Bisphenol A Epoxy Solid Resin
Weight per Epoxide (EEW, g/eq) 500 to 562. Max color is 1.Comments/Applications: Unmodified bis A "Type 2" epoxy resin. More uniform, higher flow GT 7072-type for use in powder coatings and genera..
Maximum Service Temperature, Air 75.0 - 85.0 °C
167 - 185 °F
Softening Range
Huntsman AroCy B-10 Monomeric Bisphenol-A Dicyanate
Comments/Applications: Monomeric bisphenol-A dicyanate. Softening range is 75-85°C. Filament winding, pultrusion, reactive diluent for high viscosity cyanate ester products.Data provided by Cib..
Maximum Service Temperature, Air -30.0 - 85.0 °C
-22.0 - 185 °F
SMAC SMACARCH® 1236S Damping Material
Specifications - Shock & vibration insulation for:Electronic equipment from high shock inputsShipping containers, pallets and skidsRack and chassis mounted COTS electronicsAdvantages:Large deflectio..
Maximum Service Temperature, Air -40.0 - 85.0 °C
-40.0 - 185 °F
SMAC SMACMOUNT® 1242S Damping Material
Specifications - Suspension for :Aircraft avionics components and subassembliesMissile electronicsVehicular electronics requiring vibration isolationAdvantages :Bushing style mountCountersunk for lo..