Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 324 °C | 615 °F | |
Greene Tweed CHEMRAZ® 615 Perfluoroelastomer Greene Tweed’s Chemraz® 615 exhibits outstanding high temperature properties, with a temperature range from 0°F to 615°F (-18°C to 324°C). Chemraz 615’s chemical resistance.. |
|||
Maximum Service Temperature, Air | 324 °C | 615 °F | |
Greene Tweed CHEMRAZ® 618 Perfluoroelastomer Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r.. |
|||
Maximum Service Temperature, Air | 324 °C | 615 °F | |
Greene Tweed CHEMRAZ® 653 Perfluoroelastomer Chemraz® is a black perfluoroelastomer specifically formulated to meet the extreme demands of diffusion, LPCVD and thin dry processing applications. It exhibits superior compression set resistan.. |