Greene Tweed CHEMRAZ® 615 Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Greene Tweed
Trade Name CHEMRAZ®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed CHEMRAZ® 615 Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Greene Tweed’s Chemraz® 615 exhibits outstanding high temperature properties, with a temperature range from 0°F to 615°F (-18°C to 324°C). Chemraz 615’s chemical resistance and low compression set characteristics combine to outperform tin-cured perfluoroelastomers.Chemraz 615 shows lower compression set at high temperatures and higher retained sealing force than other perfluoroelastomers available.Because Chemraz 615 allows for the use of higher process operating temperatures, it is ideal for a range of markets, from chemical process to petroleum refining. This superior perfluoroelastomer performs well in a variety of fluids such as inorganic and organic chemicals, acids, reagents, heat transfer fluids and hydrocarbons.Chemraz 615 is available in standard O-rings and custom shapes for a range of equipment, from pumps and valves to agitators and mixers, from mechanical seals and process control instruments to heat exchangers and diagnostic equipment.Applications:Mechanical sealsProcess control instrumentsHeat exchangersValvesAgitators & mixersPumpsCouplingsInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 2.02 g/cc
2.02 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength at Break 11.7 MPa
1700 psi
ASTM D1414
Tensile Strength, Yield 2.76 MPa
400 psi
@50% Elongation; ASTM D1414
6.89 MPa
1000 psi
@100% Elongation; ASTM D1414
Elongation at Break 170 %
170 %
ASTM D1414
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 324 °C
615 °F
Minimum Service Temperature, Air -17.8 °C
0.000 °F
Descriptive Properties Value Comments
Color Black