Greene Tweed CHEMRAZ® 618 Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Greene Tweed
Trade Name CHEMRAZ®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed CHEMRAZ® 618 Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical resistance approaching that of PTFE. Chemraz designs last longer and seal better in harsh environments at a wider range of temperatures than any other elastomer on the market. Chemraz solves some of the most difficult sealing problems encountered in many industries while delivering outstanding in-use cost effectiveness through custom components.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.99 g/cc
1.99 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
After 70hrs @347°F in AMS 3021
75
75
ASTM D2240
Tensile Strength at Break 13.27 MPa
1925 psi
ASTM D1414
13.80 MPa
2002 psi
After 70hrs @347°F in AMS 3021
Tensile Strength, Yield 2.55 MPa
370 psi
@50% Elongation; ASTM D1414
8.791 MPa
1275 psi
@100% Elongation; ASTM D1414
Elongation at Break 126 %
126 %
After 70hrs @347°F in AMS 3021
130 %
130 %
ASTM D1414
Compression Set 16 %
16 %
70 hours @ 446°F; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 324 °C
615 °F
Minimum Service Temperature, Air -17.8 °C
0.000 °F
Shrinkage -0.400 %

@Temperature 175 °C,
Time 252000 sec
-0.400 %

@Temperature 347 °F,
Time 70.0 hour
in AMS 3021
Descriptive Properties Value Comments
Color Black