GrafTech GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material

Category Carbon , Graphite
Manufacturer GrafTech International
Trade Name GRAFOIL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GrafTech GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GRAFOIL® GTA premium flexible graphite is a non-inhibited grade developed for use in nuclear or semiconductor applications. It is certified to meet the most rigorous purity specifications of the nuclear industry, including the General Electric Nuclear Nonmetallic Material Specification D50YP12 (Rev 2) and is typically 99.8% graphite.
Physical Properties Metric English Comments
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard
Thickness 130 microns
5.12 mil
Standard
250 microns
9.84 mil
Standard
380 microns
15.0 mil
Standard
510 microns
20.1 mil
Standard
640 microns
25.2 mil
Standard
760 microns
29.9 mil
Standard
Ash 0.20 %
0.20 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 450 °C
842 °F
Maximum Service Temperature, Inert 3000 °C
5430 °F
Minimum Service Temperature, Air -240 °C
-400 °F
Component Elements Properties Metric English Comments
Aluminum, Al 0.0015 %
0.0015 %
Carbon, C 99.8 %
99.8 %
Copper, Cu <= 0.0010 %
<= 0.0010 %
Mercury, Hg <= 0.000050 %
<= 0.000050 %
Phosphorous, P 0.0030 %
0.0030 %
Sulfur, S 0.045 %
0.045 %
Chemical Properties Metric English Comments
Ionic Impurities - Cl (Chloride) <= 10 ppm
<= 10 ppm
Leachable
Descriptive Properties Value Comments
Total Chlorides (%) <50
Total Fluorides (ppm) <10
Total Halogens (ppm) 40
Total Nitrates (ppm) 10
Total Nitrites (ppm) 1