Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 228 °C | 442 °F | Heat Resistance; ASTM D570D |
Plenco 08112 Polyester BMC, Compression Molded PLENCO 08112 is a renumber of PlasGlas 10112. PLENCO 08112 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co.. |
|||
Maximum Service Temperature, Air | 228 °C | 442 °F | Heat Resistance; ASTM D570D |
Plenco 6401 Phenolic, Briquette, Transfer Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |